Use of electric arc furnace slag for producing concrete paving blocks

In this study the electric arc furnace slag was used as coarse natural aggregate substitute in concrete paving blocks production. The concrete mixture was defined by using weight proportions in the ratio of 1:2:3:0.51 (cement:sand:coarse aggregate:water) in order to obtain a compressive strength of...

全面介紹

Saved in:
書目詳細資料
Main Authors: Penteado, Carmenlucia Santos Giordano, Evangelista, Beatriz Leão, Ferreira, Gisleiva Cristina dos Santos, Borges, Pedro Henrique Andrade, Lintz, Rosa Cristina Cecche
格式: Online
語言:eng
出版: ANTAC - Associação Nacional de Tecnologia do Ambiente Construído 2019
在線閱讀:https://seer.ufrgs.br/ambienteconstruido/article/view/78783
標簽: 添加標簽
沒有標簽, 成為第一個標記此記錄!
實物特徵
總結:In this study the electric arc furnace slag was used as coarse natural aggregate substitute in concrete paving blocks production. The concrete mixture was defined by using weight proportions in the ratio of 1:2:3:0.51 (cement:sand:coarse aggregate:water) in order to obtain a compressive strength of 35 MPa. Four groups of concrete were prepared: a reference recipe and three others with the slag replacing the natural aggregate in the proportions of 25%, 50% and 75%. The compressive strength was not influenced by the slag content; however, it was influenced by the curing age, as the sample with 75% of slag addition had its compressive strength increased by 13.5% from 7 to 56 days. Water absorption presented a slightly reduction with slag addition. The results of compressive strength and water absorption met the Brazilian technical requirements, making the paving blocks suitable for use in light vehicle traffic. The results obtained in this study highlight the influence of the production process in the final quality of the steel slag, and the need of stablishing technical and environmental requirements to guide and promote the safe use of electric arc furnace slag in concrete.